Polymer Property : Ionic Impurities - Cl (Chloride) = 34 ppm Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) 34 ppm
34 ppm
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
Ionic Impurities - Cl (Chloride) 34 ppm
34 ppm
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..