Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Cl (Chloride) | 175 ppm | 175 ppm | |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |