Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Cl (Chloride) | 169 ppm | 169 ppm | |
Epoxy Technology EPO-TEK® ED1020 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Its unique features include exce.. |
|||
Ionic Impurities - Cl (Chloride) | 169 ppm | 169 ppm | |
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |