Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Cl (Chloride) | 102 ppm | 102 ppm | |
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a .. |