Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Cl (Chloride) | <= 1000 ppm | <= 1000 ppm | |
Indium Corp. Ga2O3 Gallium Sesquioxide Synonyms: Gallium Oxide, Gallium (III) OxideCAS Number: 12024-21-4EC Number: 234-691-7RTECS: LW9650000Purity: 99.99 to 99.999% Gallium SesquioxideAppearance/Form: White powderCrystal structure.. |