Material Notes:
Synonyms: Gallium Oxide, Gallium (III) OxideCAS Number: 12024-21-4EC Number: 234-691-7RTECS: LW9650000Purity: 99.99 to 99.999% Gallium SesquioxideAppearance/Form: White powderCrystal structure: Predominantly B Phase, Confirmed by XRD AnalysisSolubility: Soluble in Alkalis. Slightly Soluble in Hot Acids. Insoluble in Water.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Apparent Density
Density 6.44 g/cc
0.233 lb/in³
Solid
Loss On Ignition <= 0.10 %

@Temperature 800 °C
<= 0.10 %

@Temperature 1470 °F
Particle Mesh Size -325 Mesh
-325 Mesh
-100 Mesh
-100 Mesh
Molecular Weight 187.44 g/mol
187.44 g/mol
Maximum Moisture Content <= 0.10

@Temperature 104 °C
<= 0.10

@Temperature 219 °F
LOD
Thermal Properties Metric English Comments
Melting Point 1900 °C
3450 °F
Component Elements Properties Metric English Comments
Chromium, Cr <= 0.00010 %
<= 0.00010 %
typical
<= 0.00030 %
<= 0.00030 %
Copper, Cu <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Gallium, Ga 0.74393 %
0.74393 %
Theoretical
Indium, In <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Iron, Fe <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Lead, Pb <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Nickel, Ni <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Sodium, Na <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Tin, Sn <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Trace Metals <= 0.00030 %
<= 0.00030 %
Total combined metals, typical
<= 0.0010 %
<= 0.0010 %
Total combined metals
Zinc, Zn <= 0.00010 %
<= 0.00010 %
Typical
<= 0.00030 %
<= 0.00030 %
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 1000 ppm
<= 1000 ppm