Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | |
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | TF, REG Powders |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | |
Ferro IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: TF Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
Ionic Impurities - K (Potassium) | 10 ppm | 10 ppm | |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Ionic Impurities - K (Potassium) | 10 ppm | 10 ppm | |
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi.. |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | AOD-S |
Dow VORANOL™ CP 755 Polyol VORANOL™ CP 755 polyol is a glycerine propoxylated polyether triol.Information provided by Dow |
|||
Ionic Impurities - K (Potassium) | <= 10 ppm | <= 10 ppm | AOD-S |
Dow VORANOL™ CP 450 Polyol VORANOL™ CP 450 polyol is a glycerine propoxylated polyether triol.Information provided by Dow |