Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Na (Sodium) | 23 ppm | 23 ppm | |
Epoxy Technology EPO-TEK® B912-8 Epoxy Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot.. |
|||
Ionic Impurities - Na (Sodium) | 23 ppm | 23 ppm | |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |