Polymer Property : Critical Temperature = 857 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 857 °C
1570 °F
Ac3
Latrobe TNWâ„¢ ASTM M10 High Speed Steel
TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2% vanadium content. TNW is popul..