Chemical Properties Metric English Comments
Critical Temperature 853 °C
1570 °F
Ar1
Latrobe LSSâ„¢ 2367 Hot Work Tool Steel
TLS 2367 is a chromium-molybdenum hot work steel that is similar to AISI H11 hot work steel, but which contains a higher molybdenum content. The higher molybdenum gives TLS 2367 better hot hardness ..
Critical Temperature 854 °C
1570 °F
Ac3
Latrobe DuraTechâ„¢ T15 Powder Metal High Speed Steel (ASTM T15)
DuraTech T15 powder metallurgy high speed steel is cobalt-bearing super high speed steel which can be heat treated to a hardness as high as 67 Rockwell C. A high volume of hard vanadium carbides pro..
Critical Temperature 854 °C
1570 °F
Ac3
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel
DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous..
Critical Temperature 852 °C
1570 °F
Ac3
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11)
TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides..
Critical Temperature 857 °C
1570 °F
Ac3
Latrobe TNWâ„¢ ASTM M10 High Speed Steel
TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2% vanadium content. TNW is popul..
Critical Temperature 854 °C
1570 °F
Ac1
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service ..