Polymer Property : Critical Temperature = 843 °C Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 843 °C
1550 °F
Ac1
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14)
TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening steel that exh..
Critical Temperature 843 °C
1550 °F
Crucible Steel WR-95 Tool Steel, AISI H10 Modified
WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight..