Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 730 °C | 1350 °F | Ar1 |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |
|||
Critical Temperature | 730 °C | 1350 °F | Ar3 |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |