Polymer Property : Linear Mold Shrinkage, Flow = 0.015 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm

@Time 86400 sec
0.013 - 0.015 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm

@Time 86400 sec
0.013 - 0.015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm

@Time 86400 sec
0.013 - 0.015 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific)
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm

@Time 86400 sec
0.013 - 0.015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific)
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.