Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0068 cm/cm

@Time 86400 sec
0.0068 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS
LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear.
Linear Mold Shrinkage, Flow 0.0068 cm/cm

@Time 86400 sec
0.0068 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific)
LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.