Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0068 cm/cm @Time 86400 sec |
0.0068 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Linear Mold Shrinkage, Flow | 0.0068 cm/cm @Time 86400 sec |
0.0068 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |