Polymer Property : Linear Mold Shrinkage, Flow = 0.0061 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0061 cm/cm

@Time 86400 sec
0.0061 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
Linear Mold Shrinkage, Flow 0.0061 cm/cm

@Time 86400 sec
0.0061 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0061 cm/cm

@Time 86400 sec
0.0061 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66
LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive.