Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0054 cm/cm @Time 86400 sec |
0.0054 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0054 cm/cm @Time 86400 sec |
0.0054 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0054 cm/cm @Time 86400 sec |
0.0054 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Linear Mold Shrinkage, Flow | 0.0054 cm/cm @Time 86400 sec |
0.0054 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |