Polymer Property : Linear Mold Shrinkage, Flow = 0.0027 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES
LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66
LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66
LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66
LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region...
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MV006SU PP
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MV006SU PP (Asia Pacific)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MV006SU PP (Europe-Africa-Middle East)
LNP VERTON* MV006SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific)
LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific)
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MX02795 PP
LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural.