Polymer Property : Linear Mold Shrinkage, Flow = 0.0014 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0014 - 0.0019 cm/cm

@Time 86400 sec
0.0014 - 0.0019 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..
Linear Mold Shrinkage, Flow 0.0014 - 0.0016 cm/cm

@Thickness 1.00 mm
0.0014 - 0.0016 in/in

@Thickness 0.0394 in
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Linear Mold Shrinkage, Flow 0.0014 cm/cm

@Time 86400 sec
0.0014 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific)
LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0014 - 0.0019 cm/cm

@Time 86400 sec
0.0014 - 0.0019 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant.
Linear Mold Shrinkage, Flow 0.0014 - 0.0019 cm/cm

@Time 86400 sec
0.0014 - 0.0019 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific)
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0014 cm/cm

@Time 86400 sec
0.0014 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea..
Linear Mold Shrinkage, Flow 0.0014 cm/cm

@Time 86400 sec
0.0014 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific)
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System.
Linear Mold Shrinkage, Flow 0.0014 cm/cm

@Time 86400 sec
0.0014 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE0049P PC
LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct..
Linear Mold Shrinkage, Flow 0.0014 - 0.0019 cm/cm

@Time 86400 sec
0.0014 - 0.0019 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific)
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..