Polymer Property : Linear Mold Shrinkage, Flow = 0.0012 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Time 86400 sec
0.0012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC
LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by..
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Time 86400 sec
0.0012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Time 86400 sec
0.0012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.