Physical Properties | Metric | English | Comments |
---|---|---|---|
Solubility | 10 ppm | 10 ppm | H<sub>2</sub>, by weight, at 760 mm Hg/25°C |
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally .. |