Polymer Property : Vapor Pressure = 50.0 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0667 bar

@Temperature 121 °C
50.0 torr

@Temperature 250 °F
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam ..
Vapor Pressure 0.0667 bar

@Temperature 260 °C
50.0 torr

@Temperature 500 °F
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally ..
Vapor Pressure 0.0667 bar

@Temperature 350 °C
50.0 torr

@Temperature 662 °F
ChevronTexaco 22 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Vapor Pressure 0.0667 bar

@Temperature 180 °C
50.0 torr

@Temperature 356 °F
AboCure
Abatron AboCast/AboCure 8109-5
High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications..
Vapor Pressure 0.0667 bar

@Temperature 180 °C
50.0 torr

@Temperature 356 °F
AboCure
Abatron AboCast/AboCure 8109-6
High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat..