Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00456 bar @Temperature 0.000 °C |
3.42 torr @Temperature 32.0 °F |
19 g/m<sup>3</sup> concentration of saturated vapor |
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |