Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000933 bar @Temperature 80.0 °C |
0.700 torr @Temperature 176 °F |
AboCure |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |