Polymer Property : Vapor Pressure = 0.129 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.129 bar

@Temperature 135 °C
96.5 torr

@Temperature 275 °F
Dow Hydroxyethyl Acrylate
Hydroxethyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow