Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.126 bar @Temperature 60.0 °C |
94.2 torr @Temperature 140 °F |
420 g/m<sup>3</sup> concentration of saturated vapor |
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |