Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0122 bar @Temperature 15.0 °C |
9.12 torr @Temperature 59.0 °F |
47 g/m<sup>3</sup> concentration of saturated vapor |
Solvay Chemicals Epichlorohydrin Epichlorohydrin is a chemical intermediate, mainly dedicated to the manufacturing of epoxy resins used in Paints & coatings, Composites, Adhesives and Electronics. It is also used in non-epoxy appli.. |