Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000440 bar @Temperature 25.0 °C |
0.330 torr @Temperature 77.0 °F |
|
Dow Glycidyl Methacrylate Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow |