Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow
Physical Properties Metric English Comments
Density 1.068 g/cc
0.03858 lb/in³
1.03 g/cc

@Temperature 66.0 °C
0.0372 lb/in³

@Temperature 151 °F
Viscosity 2.7 cP

@Temperature 15.5 °C
2.7 cP

@Temperature 59.9 °F
Molecular Weight 142.15 g/mol
142.15 g/mol
Maximum Moisture Content 0.15
0.15
wt% water
Vapor Pressure 0.000440 bar

@Temperature 25.0 °C
0.330 torr

@Temperature 77.0 °F
0.149 bar

@Temperature 135 °C
112 torr

@Temperature 275 °F
Thermal Properties Metric English Comments
Melting Point <= -70.0 °C
<= -94.0 °F
Boiling Point 189 °C
372 °F
760 mm Hg
Flammability Test 1.1
1.1
[mole %] Lower Flammability Limit @ 100°C
Flash Point 85.0 °C
185 °F
PMCC
Optical Properties Metric English Comments
Refractive Index 1.4473
1.4473
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm