Density 0.933 g/cc

@Temperature 60.0 °C
0.0337 lb/in³

@Temperature 140 °F
BASF Pluracol® 1062 Specialty Polyol
Description: Pluracol® 1062 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 1062 can also be use..