Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.933 g/cc @Temperature 60.0 °C |
0.0337 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 1062 Specialty Polyol Description: Pluracol® 1062 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 1062 can also be use.. |