Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.10 - 1.20 g/cc @Temperature 25.0 °C |
0.0397 - 0.0434 lb/in³ @Temperature 77.0 °F |
RTM 120 bisphenol epoxy resin containing reactive diluent; ISO 1675 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Density | 1.10 g/cc @Temperature 43.3 °C |
0.0397 lb/in³ @Temperature 110 °F |
|
BASF Pluracol® 1158 Specialty Polyol Description: Pluracol® 1158 polyol is a polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. Wh.. |
|||
Density | 1.10 g/cc @Temperature 60.0 °C |
0.0397 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® SG-470 Rigid Polyol Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |
|||
Density | 1.10 g/cc @Temperature 25.0 °C |
0.0397 lb/in³ @Temperature 77.0 °F |
Liquid |
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Density | 1.10 g/cc @Temperature 60.0 °C |
0.0397 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® 735 Rigid Polyol Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Fo.. |
|||
Density | 1.10 g/cc @Temperature 60.0 °C |
0.0397 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® SG-450 Rigid Polyol Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |