Material Notes:
Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Formulations containing Pluracol 735 may be utilized for foaming insulated panels, refrigerators, coolers, doors, or decorative moldings by either pour-in-place or frothing techniques. Pluracol 735 has good compatibility with common foam ingredients. It improves the processability and decreases the friability of many low density foam formulations. Pluracol 735 is not recommended for use in quasi-prepolymer preparations nor for use as the sole polyol component in the preparation of foams.Information provided by BASF
Physical Properties Metric English Comments
Density 1.10 g/cc

@Temperature 60.0 °C
0.0397 lb/in³

@Temperature 140 °F
1.12 g/cc

@Temperature 40.0 °C
0.0405 lb/in³

@Temperature 104 °F
1.15 g/cc

@Temperature 25.0 °C
0.0415 lb/in³

@Temperature 77.0 °F
Viscosity 415 cP

@Temperature 60.0 °C
415 cP

@Temperature 140 °F
2300 cP

@Temperature 40.0 °C
2300 cP

@Temperature 104 °F
5500 cP

@Temperature 25.0 °C
5500 cP

@Temperature 77.0 °F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Brown Liquid
Hydroxyl Number 438 - 465 mg KOH/g
STI 3007/3162