Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.009 g/cc @Temperature 0.000 °C |
0.03645 lb/in³ @Temperature 32.0 °F |
Concentration 0.01 kg FeCl3/kg |
Solvay Chemicals Ferric chloride Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay |
|||
Density | 1.009 g/cc @Temperature 100 °C |
0.03645 lb/in³ @Temperature 212 °F |
Concentration 0.10 kg HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |