Polymer Property : Density = 0.0307 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.851 g/cc

@Temperature 37.8 °C
0.0307 lb/in³

@Temperature 100 °F
Duratherm 450 Paraffinic Heat Transfer Fluid
Duratherm 450 - thermal fluid specifically engineered for applications requiring process heating and cooling efficiently between 30°F and 450°F. Economical and thermally stable, Duratherm 450 offe..
Density 0.851 g/cc

@Temperature 37.8 °C
0.0307 lb/in³

@Temperature 100 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..