Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.731 g/cc @Temperature 121 °C |
0.0264 lb/in³ @Temperature 250 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Density | 0.731 g/cc @Temperature 65.6 °C |
0.0264 lb/in³ @Temperature 150 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Density | 0.731 g/cc @Temperature 204 °C |
0.0264 lb/in³ @Temperature 400 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Density | 0.732 g/cc @Temperature 204 °C |
0.0264 lb/in³ @Temperature 400 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |
|||
Density | 0.731 g/cc @Temperature 260 °C |
0.0264 lb/in³ @Temperature 500 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |
|||
Density | 0.732 g/cc @Temperature 204 °C |
0.0264 lb/in³ @Temperature 400 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |