Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.650 g/cc @Temperature 22.0 °C |
0.0235 lb/in³ @Temperature 71.6 °F |
Cure Cycle: 5 days at 22°C; ASTM D792 |
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu.. |
|||
Density | 0.650 g/cc @Temperature 316 °C |
0.0235 lb/in³ @Temperature 600 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |