Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 2.10 - 510 g/l
2.10 - 510 g/l
Average value: 222 g/l Grade Count:13
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..