Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Volatile Organic Compounds (VOC) Content | 431 g/l | 431 g/l | |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |