Polymer Property : Volatile Organic Compounds (VOC) Content = 100 g/l Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 100 g/l
<= 100 g/l
Dow Corning IE 6694 WATER REPELLENT
Dow Corning IE-6694 Water Repellent Emulsion is a 60% active, water-dilutable silicone water repellent that imparts penetrating water repellency for treatment of concrete, masonry and stone construc..
Volatile Organic Compounds (VOC) Content 100 g/l
100 g/l
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).