Polymer Property : Storage Temperature = 26.7 °C Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Storage Temperature 4.44 - 26.7 °C
40.0 - 80.0 °F
Hexcel® Redux® 108 Surface Pretreatment Protection Solution
The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co..
Storage Temperature 4.44 - 26.7 °C
40.0 - 80.0 °F
Hexcel® Redux® 112 Surface Pretreatment Protection Solution
The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co..
Storage Temperature 4.44 - 26.7 °C
40.0 - 80.0 °F
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..