Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 50 cP | 50 cP | ASTM D789 |
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Relative Viscosity | 50 cP | 50 cP | ASTM D789 |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Relative Viscosity | 50 cP | 50 cP | ASTM D789 |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Relative Viscosity | 50 cP | 50 cP | ASTM D789 |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Relative Viscosity | 50 cP | 50 cP | ASTM D789 |
Clariant Renol 6001 GP HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Relative Viscosity | 50 cP | 50 cP | |
Clariant Renol N6 15% Moly MOS2 Concentrate of Molybdenum Disulfide Application to Nylon 6, Nylon 66Data provided by Clariant Masterbatches |
|||
Relative Viscosity | 50 - 54 cP | 50 - 54 cP | Formic Acid; ASTM D789 |
Ascend Performance Materials Vydyne® 52BWMS Nylon 66 Vydyne® 52BWMS is a medium-viscosity resin used for extrusion-compounding. It is the product of choice for low-yellowness-required applications. This product with its higher viscosity is a part of .. |