Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 4.1 cP | 4.1 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 43 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 43 is a non-chain modified ultra-high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical properties, fo.. |
|||
Relative Viscosity | 4.1 cP | 4.1 cP | 98% H2SO4 |
UBE 5034FDX17 Air Blown Nylon 6/66 Film Specialties: Special grade for Air blownLow curlHigh transparencyHigh shrinkGood thermoform-abilityApplications: Best for Air BlownProcessing: Pouch (Air blown)Information provided by UBE. |
|||
Relative Viscosity | 4.1 - 4.3 cP | 4.1 - 4.3 cP | 98% H2SO4 |
UBE 5034FDX33 Air Blown Nylon 6/66 Film Specialties: High transparencyLow neck-inNucleated typeApplications: Suitable for T-die,Water and Air blown process Processing: Shrink bags (Water) Pouch ( Air blown) Information provided by UBE. |