Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.95 - 4.05 cP | 3.95 - 4.05 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 40 Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Relative Viscosity | 3.95 - 4.05 cP | 3.95 - 4.05 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ E 40 LN Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Relative Viscosity | 3.95 - 4.05 cP | 3.95 - 4.05 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ E 40 T Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Relative Viscosity | 3.95 - 4.05 cP | 3.95 - 4.05 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ E 40 L Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |