Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Relative Viscosity = 3.95 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Relative Viscosity 3.95 - 4.05 cP
3.95 - 4.05 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 40 Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.95 - 4.05 cP
3.95 - 4.05 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 40 LN Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.95 - 4.05 cP
3.95 - 4.05 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 40 T Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Relative Viscosity 3.95 - 4.05 cP
3.95 - 4.05 cP
1% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ E 40 L Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™