Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.8 cP | 3.8 cP | 96% H2SO4 |
UBE 5034FDX17 Air Blown Nylon 6/66 Film Specialties: Special grade for Air blownLow curlHigh transparencyHigh shrinkGood thermoform-abilityApplications: Best for Air BlownProcessing: Pouch (Air blown)Information provided by UBE. |
|||
Relative Viscosity | 3.8 - 3.98 cP | 3.8 - 3.98 cP | 96% H2SO4 |
UBE 5034FDX33 Air Blown Nylon 6/66 Film Specialties: High transparencyLow neck-inNucleated typeApplications: Suitable for T-die,Water and Air blown process Processing: Shrink bags (Water) Pouch ( Air blown) Information provided by UBE. |