Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 3.38 - 3.5 cP | 3.38 - 3.5 cP | 96% H2SO4 |
UBE 1024FDX41 Nylon 6 BOPA Film Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE. |