Relative Viscosity 3.38 - 3.5 cP
3.38 - 3.5 cP
96% H2SO4
UBE 1024FDX41 Nylon 6 BOPA Film
Specialties: Excellent processing stabilityProcessing: Best for BOPAApplications: BOPA film (T-die)Information provided by UBE.