Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.25 cP | 2.25 cP | QC-10-104 |
Formosa Plastics Formolon® 34 PVC PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t.. |
|||
Relative Viscosity | 2.25 cP | 2.25 cP | QC-10-104 |
Formosa Plastics Formolon® KVF PVC PVC Homopolymer Dispersion Resin F-KVF is a medium molecular weight, fine particle PVC homopolymer dispersion which imparts pesudoplastic flow to plastisol in which it is used. Plastisol prepared ut.. |