Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.15 cP | 2.15 cP | QC-10-104 |
Formosa Plastics Formolon® 24A PVC PVC Homopolymer Dispersion Resin F-24A is a low molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compounds as well as other applica.. |
|||
Relative Viscosity | 2.15 cP | 2.15 cP | |
Formosa Plastics Formolon® 622E PVC Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry.. |
|||
Relative Viscosity | 2.15 cP | 2.15 cP | |
Formosa Plastics Formolon® 622S PVC Homopolymer Siding Grade Resin F622S is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications, but it is also suitable for many flexible applications. Thi.. |